  【塑料球】塑料空心球,塑胶球价格,塑料小球生产厂家POM塑料球(POM塑胶球)PA塑料球(尼龙塑料球)PP塑料球(塑料PP球)PMMA塑料球(PMMA塑胶球)PC塑料球(PC塑胶球)PVC塑料球(PVC塑胶球)PPA塑料球(PPA塑胶球)PSU塑料球(PSU塑胶球)玩具塑料球(儿童玩具球)饰品塑料球(饰品塑胶球)塑料空心球(空心塑胶球)生物降解塑料球(PLA塑料球)软胶塑料球(软胶塑胶球)PEEK塑料球(PEEK塑胶球)PTFE塑料球(特氟龙塑料球)TPX塑料球(TPX塑胶球)Pepper ball0.68 Pepperball塑料焊接技术解决方案塑料热板焊接技术塑料超声波焊接技术塑料激光焊接技术塑料摩擦焊接技术实心塑料球(实心塑胶球)POM实心塑料球(POM塑料球)PA实心塑料球(PA塑料球)实心PP塑料球(塑料PP球)PMMA实心塑料球(PMMA塑料球)PVC实心塑料球(PVC塑料球)PTFE实心塑料球(特氟龙塑料球)塑料小球,塑料小球厂家精密塑料球焊接技术解决方案塑料激光焊接实用技术塑料热板焊接实用技术塑料超声焊接实用技术塑料球行业新闻,塑胶球新闻塑料空心球(空心塑料球)PTFE空心塑料球(PTFE空心球)PC空心塑料球(PC空心球)POM空心塑料球(POM塑料球)TPX空心塑料球(TPX空心球)PP空心塑料球(塑料空心PP球)PA空心塑料球(PA空心球)塑料浮球(塑胶浮球)PE空心球塑料球规格,塑胶球规格游戏塑料球,游戏塑胶球塑料空心球规格,空心塑胶球规格塑胶球标准,塑料球标准塑料空心球标准,空心塑胶球标准塑料球规格尺寸,塑胶规格尺寸塑料球硬度测试方法,塑胶球测试空心塑料球密度测试方法塑胶球规格,塑料球规格橡胶球,硅胶球,橡胶球价格,硅胶球厂家橡胶球-硅胶球厂家硅胶球,食品级硅胶球硅胶洗衣球-硅胶球厂家橡胶洗衣球-硅胶球厂家空心硅胶球,空心橡胶球橡胶弹力球橡胶球规格,硅胶球规格橡胶密封圈塑料球阀电动塑料球阀(电动塑胶球阀)塑料浮球阀(塑胶浮球阀)塑料法兰球阀(塑胶法兰球阀)氟塑料球阀(氟塑胶球阀)塑料三通球阀(塑胶三通球阀)胡椒球,胡椒弹0.43英寸塑料彩弹0.68英寸塑料彩弹0.68英寸胡椒球Pepper ball0.68 pepper ball0.50 pepper ball taiwan0.43 peper ball japanBB弹
产品简介 首页 > 产品简介 >  
 
 
Quality control of plastic hollow pepper ball blow molding
 
 
 
详情
 

Plastic hollow pepper balls are made by blow molding process, and compressed air is used in the blow molding process. The pressure and temperature of compressed air have great influence on the quality of plastic hollow pepper balls. If the pressure exceeds a certain value, it will cause the phenomenon of plastic hollow pepper balls lacking glue and less glue.

Generally speaking, when processing plastic hollow pepper balls by blow molding machine, the pressure should be within 3kPa. If it exceeds this pressure, the pressure will be too high, which will cause the wall thickness of plastic hollow pepper balls to be inconsistent. One side of the wall thickness is too thin and the other side is too thick, and the strength of plastic hollow pepper balls is not enough, which will not only affect the appearance of plastic hollow pepper balls, but also affect the strength of plastic hollow pepper balls.

The second point is the temperature of compressed air. Plastic hollow pepper balls need temperature for molding. If the compressed hollow temperature used for blow molding is too low, the melted plastic material will be cooled rapidly and cannot be molded at all. Therefore, when the plastic hollow pepper balls are manufactured by the blow molding machine, the temperature of compressed air must be above 80 degrees. Only in this way can the normal operation of the blow molding machine be guaranteed and the quality of plastic hollow pepper balls can be guaranteed.



 