  【塑料球】塑料空心球,塑胶球价格,塑料小球生产厂家POM塑料球(POM塑胶球)PA塑料球(尼龙塑料球)PP塑料球(塑料PP球)PMMA塑料球(PMMA塑胶球)PC塑料球(PC塑胶球)PVC塑料球(PVC塑胶球)PPA塑料球(PPA塑胶球)PSU塑料球(PSU塑胶球)玩具塑料球(儿童玩具球)饰品塑料球(饰品塑胶球)塑料空心球(空心塑胶球)生物降解塑料球(PLA塑料球)软胶塑料球(软胶塑胶球)PEEK塑料球(PEEK塑胶球)PTFE塑料球(特氟龙塑料球)TPX塑料球(TPX塑胶球)Pepper ball0.68 Pepperball塑料焊接技术解决方案塑料热板焊接技术塑料超声波焊接技术塑料激光焊接技术塑料摩擦焊接技术实心塑料球(实心塑胶球)POM实心塑料球(POM塑料球)PA实心塑料球(PA塑料球)实心PP塑料球(塑料PP球)PMMA实心塑料球(PMMA塑料球)PVC实心塑料球(PVC塑料球)PTFE实心塑料球(特氟龙塑料球)塑料小球,塑料小球厂家精密塑料球焊接技术解决方案塑料激光焊接实用技术塑料热板焊接实用技术塑料超声焊接实用技术塑料球行业新闻,塑胶球新闻塑料空心球(空心塑料球)PTFE空心塑料球(PTFE空心球)PC空心塑料球(PC空心球)POM空心塑料球(POM塑料球)TPX空心塑料球(TPX空心球)PP空心塑料球(塑料空心PP球)PA空心塑料球(PA空心球)塑料浮球(塑胶浮球)PE空心球塑料球规格,塑胶球规格游戏塑料球,游戏塑胶球塑料空心球规格,空心塑胶球规格塑胶球标准,塑料球标准塑料空心球标准,空心塑胶球标准塑料球规格尺寸,塑胶规格尺寸塑料球硬度测试方法,塑胶球测试空心塑料球密度测试方法塑胶球规格,塑料球规格橡胶球,硅胶球,橡胶球价格,硅胶球厂家橡胶球-硅胶球厂家硅胶球,食品级硅胶球硅胶洗衣球-硅胶球厂家橡胶洗衣球-硅胶球厂家空心硅胶球,空心橡胶球橡胶弹力球橡胶球规格,硅胶球规格橡胶密封圈塑料球阀电动塑料球阀(电动塑胶球阀)塑料浮球阀(塑胶浮球阀)塑料法兰球阀(塑胶法兰球阀)氟塑料球阀(氟塑胶球阀)塑料三通球阀(塑胶三通球阀)胡椒球,胡椒弹0.43英寸塑料彩弹0.68英寸塑料彩弹0.68英寸胡椒球Pepper ball0.68 pepper ball0.50 pepper ball taiwan0.43 peper ball japanBB弹
产品简介 首页 > 产品简介 >  
 
 
Causes of bubbles in the middle of plastic PP pepper ball
 
 
 
详情
 

Plastic PP pepper balls are transparent, and it is easy to see bubbles in the middle. Some customers have high quality requirements and do not accept plastic PP pepper balls with bubbles in the middle. The reason for the bubbles in plastic PP pepper balls is mainly formed in the injection molding process, so the improvement direction is to improve the design method of the mold besides the injection molding process.

Bubble caused by material: The material contains moisture. When it is used as an ordinary plastic product, it is thinner than the product and will not produce bubbles. However, the wall thickness of plastic PP pepper balls is generally more than 5mm, and the cavity is large, so the gas can not be discharged at all. Therefore, the material must be dried before injection molding.

Bubble caused by mold: The main reason for the bubble of plastic PP pepper ball caused by mold is that the air in the mold cavity cannot be exhausted. The improvement method is to exhaust the mold, which solves the problem of plastic PP pepper ball bubble caused by poor exhaust.

Bubbles caused by the temperature of the injection molding machine: During the injection molding process, the temperature of the injection molding machine is too high, the PP material decomposes and gasifies, and some gas enters the mold with the rubber compound to form bubbles. The improvement method is to lower the temperature of the injection molding machine, generally below 215 degrees. After the temperature is lowered, the problem of plastic PP pepper ball bubbles caused by material gasification can be basically solved.


 